| Grade TG-1740 |
Specification |
Typical Result * |
Test Method |
| Binder................................................ |
SBR/NBR |
SBR/NBR |
|
| Cork Grain Size................................. |
0.5 to 1 mm |
0.5 to 1
mm |
|
Physical Characteristics
Hardness, Shore A...............................
Compressibility at 400 PSI(%)..............
Recovery after (%)...............................
Tensile Strength (Kg/cm2)................... |
70 +/- 5
25 ~ 35
80 min
12.75 min |
67.67
28.98
84.27
19.22 |
ASTM D 2240
ASTM F 36
ASTM F 36
ASTM F 152 |
| Flexibility (Thickness x 3) |
No Cracks |
No Cracks |
ASTM F 147 |
Volume Change After Immersion
ASTM no.3 Oil,70 hrs @100 deg C( %). |
40 Max |
32.39 |
ASTM F 146 |